铝 单 板
ALUMINUM VENEER
产品选材
我公司选用进口和国产优质专用铝板为基料。
板材厚度系列有1.0mm,1.5mm,2.0mm,2.5mm,3.0mm,4.0mm,5.0mm,6.0mm等。
氟碳涂料( KYNAR500):采用国际著名涂料公司授权的氟碳涂料。
产品结构
铝单板的结构主要有面板、加强筋、挂耳等部件组成。有要求时板背面可填隔热棉,挂耳可直接有面板折
弯而成,亦可在面板上另外加装。
铝单板
ALUMINUM VENEER
序号
1
2
3
4
5
6
7
8
9
10
11
12
13
14
15
16
17
18
项目
铝单板基材材料
Aluminum single plate substrate materials
铝单板基材材料符合GB/T3880-1997规定
Aluminum single plate substrate materials shall comply with the provisions of GB/T3880-1997.
铝单板长度
Aluminum single plate length
铝单板宽度
Aluminum single plate width
铝单板对角线偏差
Aluminum single plate diagonal deviation
铝单板折边高度偏差
Aluminum single plate flanging height deviation
铝单板角度
Aluminum single plate angle
铝单板平面度
Aluminum single plate flatness
外观质量
Appearance quality
涂层干膜厚度
Dry film thickness of coating
涂层颜色均匀性
Coating color uniformity
涂层铅笔硬度
Coating pencil hardness
涂层干式附着力
Dry adhesion coating
涂层湿式附着力
Wet adhesion of coating
涂层沸水附着力
Coating adhesion in boiling water
涂层抗冲击性能
lmpact resistance properties of the coating
涂层耐盐酸性能
Hydrochloric acid resistance of coating
涂层耐硝酸性能
Nitric acid resistance of coating
涂层耐洗涤剂性能
Detergent resistance of coating
Code Items
单位 标准要求
Unit Standard Renquiremernts
mm ±1.0
±1.0
<2000 +2.0
±0.40
<2
<2000 +3.0
≥1H
涂层应平滑,色泽均匀.不得有明显的流痕.皱纹、气泡、裂纹、划痕和夹杂物。或其他
影响使闸性的表面缺陷。
Coating should be smooth uniform color.no obvious scar. wrinkles,bubbles.cracks,scratchesand
inclusions or other effects of the use of surface defects.
二涂:平均膜厚30 三涂:平均膜厚40 最小局部膜厚:25 最大局部膜厚:35
The minimum local thickness:25 The maximum local film thickness:35
2nd: the average film thickness of 30 3rd: the average film thickness:40
颜色的均匀性符合供需双方认可的色板所规定的色号以及认可的色差范围。
规格法优于0级
规格试验后,在世界上38℃c -5℃蒸馏水或负离子水中浸泡24H,试验后划格区干膜
不得落霜移位。
recognized color swatches of color difference and the scope approved.
The uniformity of color should be consistent with the provisions of the supply and demand sides
Specification tests, in the world 38'c -5c distilled water or negative ions in the water to soak
for 24h. after testing a cross-cut area dry film may not fall off and shift.
规格试验后,在浸入95℃的沸水中浸泡20分钟,划格区下膜不得脱落和移位.试样
不得有气泡。
涂层经392N,cm冲击试验后,干膜应无裂痕或脱落。
途层经浓度为10的盐酸溶液试验区15分钟后.目视检查涂层试验区表面应无气泡和
可见的变化。
涂层经浓度为70的硝酸溶液试验区30分钟后.试验表面和无试验表面颜色的变化。
试样经浸入38C3洗涤剂溶液中72小时试验后,涂层干膜附着力不得降低.不得有气
泡和肉眼可见的表面变化。
Specification tests, on-the-job personnel $5'c boiling water soak tfor 20 minutes a crossoutarea dry film may not fall off and shift, the sample may not have bubble.
Coating by 392N.cm after the impact test. the dry film should be no crack or fall off.
The coating concentration of hydrochloric acid solution by experimental zone and 10 after
15minutes, visual inspection test of coated surface should be free of bubbles and visible changes.
Coating with concentration for 30 minutes after the test of 70 nitric acid solution, test surfaceand、
no experimental surface color change.
Samples with 38C3 invasion is not enough detergent solution for 72hours after the test, coating
dry filmadthesion is not reduced, there shall be no changes in surface air bubbles visible to the naked eye.
specification method better than o.
mm
mm
mm
级
Class
mm
(·)